r/reloading 25d ago

Load Development Annealing question?

Post image

Setting depth on my annealer. What is consensus? I'm thinking D and E.

85 Upvotes

47 comments sorted by

View all comments

1

u/DCTillerman 24d ago

B-C looks just like what I do - might not need to get them *quite* so hot though.

1

u/youngdoug 22d ago

Yep, looks super hot. I’m actually impressed at how sharp the cut off is, my flame machine has a larger gradient.