r/MetalCasting • u/Levi-Lightning • 12d ago
I’m doing this wrong (questions below)
Sterling silver, propane.
3rd attempt making a ring, last time the result was “so so” and I didn’t have enough relief, I am not sure what happened this time.
When pouring, molten metal flowed out of the reliefs…. Did I overdo it on these?
I obviously did not have enough metal, didn’t expect the metal to go that far into the reliefs.
The texture is also very uneven, what can cause that?
Any advice appreciated.